MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aleris Weldural Aluminum Alloy, 200 mm Thickness
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Sample treatment not specified for property data.

Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldability and machinability. Fair corrosion resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.84 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 130130
Hardness, Knoop 163163Estimated from Brinell
Hardness, Rockwell A 49.449.4Estimated from Brinell
Hardness, Rockwell B 7979Estimated from Brinell
Hardness, Vickers 149149Estimated from Brinell
Tensile Strength, Ultimate >= 370 MPa>= 53700 psiMinimum
 440 MPa63800 psiTypical
Tensile Strength, Yield  >= 270 MPa
@Strain 0.2 %
>= 39200 psi
@Strain 0.2 %
Minimum
 335 MPa
@Strain 0.2 %
48600 psi
@Strain 0.2 %
Typical
Elongation at Break >= 3.0 %>= 3.0 %Minimum
 6.5 %6.5 %Typical
Modulus of Elasticity 73.8 GPa10700 ksi
Machinability 70 %70 %
Shear Strength 259 MPa37600 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000590 ohm-cm0.00000590 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.5 µm/m-°C
@Temperature 20.0 - 100 °C
12.5 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 130 W/m-K902 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 93 %93 %
Copper, Cu 5.8 - 6.8 %5.8 - 6.8 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Manganese, Mn 0.20 - 0.40 %0.20 - 0.40 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.30 %<= 0.30 %
Titanium, Ti 0.020 - 0.10 %0.020 - 0.10 %
Zinc, Zn <= 0.10 %<= 0.10 %
Zirconium, Zr 0.10 - 0.25 %0.10 - 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2024-T4; 2024-T351
Aleris Hokotol Aluminum Alloy, 200 mm Thickness
Alclad Aluminum 2014-T6, T651
Aluminum 6013-T651
2002 Aluminum Composition Spec

NHOOG21 / 17348

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.