Beologic Beobase 10 PP cotton INJ044 Black Injection Molding
Categories:
Polymer
;
Renewable/Recycled Polymer
;
Thermoplastic
;
Polypropylene (PP)
Material Notes:
Main properties visual textile fiber, good impact-stiffness balance. Applications: industrial and consumer goods, furniture, non-food markets
Information provided by Beologic.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.930
g/cc
0.0336
lb/in³
ISO 1183-1
Melt Flow
17.8
g/10 min
@Load 16.0 kg,
Temperature 230 °C
17.8
g/10 min
@Load 35.3 lb,
Temperature 446 °F
Mechanical Properties
Metric
English
Comments
Tensile Strength
30.4
MPa
4410
psi
ISO 527-1
Elongation at Break
9.5 %
9.5 %
ISO 527-1
Tensile Modulus
1.79
GPa
260
ksi
ISO 527-1
Flexural Modulus
1.793
GPa
260.1
ksi
ISO 178
Charpy Impact Unnotched
4.48
J/cm²
21.3
ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched
0.490
J/cm²
2.33
ft-lb/in²
ISO 179-1eA
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
116
°C
241
°F
ISO 75-1 (B)
Vicat Softening Point
95.2
°C
203
°F
B120; ISO 306
Descriptive Properties
Beologic Article Number
1090050044
Carbon footprint (kg CO2 eq/kg)
1.625
PAS 2050
Natural fiber content (%)
25
Renewable content
yes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PBEOL9845 / 314131
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.