MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat resistance, impact resistance, and processability requirements of a wide range of applications.

Applications:

    Automotive: Back beam, roof molding, instrument panel, cowl vent grill, speaker frame, lamp parts, glove box housing

    Electrical and Electronic: Household appliances housings and internal parts, key top, switch, compressor terminal board, cd changer, deck items, floppy disc carriage, electric tool housing

    Industrial Parts and Household Appliance: Lawn mower housing, motor housing, pump impeller

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 49.0 MPa7110 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Flexural Strength 90.0 MPa13100 psiASTM D790
Flexural Modulus 3.23 GPa468 ksiASTM D790
Izod Impact, Notched 1.70 J/cm
@Temperature 23.0 °C
3.18 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 220 °C374 - 428 °F
Middle Barrel Temperature 220 - 240 °C428 - 464 °F
Front Barrel Temperature 230 - 250 °C446 - 482 °F
Nozzle Temperature 230 - 250 °C446 - 482 °F
Melt Temperature 230 - 250 °C446 - 482 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 3 - 4 hour3 - 4 hour
Injection Pressure 58.84 - 88.26 MPa8534 - 12800 psiSecond
 63.74 - 93.16 MPa9245 - 13510 psiFirst
Back Pressure 1.96 - 4.90 MPa284 - 711 psi
Screw Speed 70 - 100 rpm70 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMAX IN-5001 High Impact PBT
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant
Overview of materials for Polypropylene, Extrusion Grade

PLGCHEM027 / 50848

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.