LL0205KJ is linear low density polyethylene copolymer containing butene-1(C4) as comonomer. It is suitable for blending with conventional LDPE. Film made from pure LL0205KJ has the following advantages over LDPE: better sealing, higher puncher resistance, greater drowdown ability, easy opening properties in 2 layer film and higher tensile strength. Applications: green house film, silage film, heavy duty plastic bags, hand bags and general purpose film applications.Information provided by Tabriz Petrochemical Company. |