MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil 0 Mobilux EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are formulated to provide extra protection against wear, rusting and water washout. They are available in NLGI grades ranging from 00 to 3, with base oil viscosities ISO VG 150, 320 and 460. Mobilux EP 0, 1, 2, and 3 greases are recommended for most types of industrial applications including heavy-duty applications where high unit pressures or shock loads are present. These greases provide excellent protection against rust and corrosion and resist water wash-out which makes them particularly suitable for equipment where moist or wet conditions are common. Mobilux EP 0 and 1 are suitable for centralised systems. Mobilux EP 2 and 3 are general-purpose greases. The recommended operating temperature range is from -20ºC to 130ºC but they may be used at higher temperatures if the lubrication frequency is increased accordingly. Mobilux EP 023 is particularly suitable for the lubrication of enclosed gears and bearings in poorly sealed gear cases they can also be used in many other industrial applications where conventional gear oils cannot be retained in gear cases, chain cases, etc. because of leakage due to worn or missing seals. The recommended operating temperature range is -15 to 120ºC for Mobilux EP 023.

Mobilux EP 0 and EP 1 provide good low temperature pumpability and are suitable for centralised lubrication systems and other applications where low temperature performance is required.

Key Words: NLGI Grade 0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 160 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 250 kgASTM D2596
Four Ball Wear 0.400 mmASTM D2266
Penetration 370Worked, 25°C; ASTM D217
Timken Test 40.0 lb
 
Thermal PropertiesOriginal ValueComments
Dropping Point 190 °CASTM D2265
 
Descriptive Properties
Colorbrown
Rust Prevention, Distilled WaterpassASTM D665A
Soap/Thickener Typelithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Mobil Vaculine 533
ExxonMobil 7 Mobilith SHC Series
ExxonMobil 2 Mobilux EP
ExxonMobil 101 Mobilgrease EAL
ExxonMobil 100 Mobil DTE FM Series

WEXXON415 / 75840

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.