MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

ASI® MG 500 Medical Grade Cyanoacrolate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: MG500 is a medical grade instant adhesive. These products have USP Class VI certification and are used in assembling medical devices.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Viscosity 500 cP500 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.7 MPa3000 psiGrit blased steel; ASTM D 2095
Adhesive Bond Strength 1.10 MPa160 psiShear vs. Phenolic. Substrate failure.; ASTM D1002
 >= 5.69 MPa>= 825 psiShear vs. Polycarbonate. Substrate failure.; ASTM D1002
 >= 6.10 MPa>= 885 psiShear vs. ABS. Substrate failure.; ASTM D1002
 >= 6.14 MPa>= 890 psiShear vs. PVC. Substrate failure.; ASTM D1002
 >= 11.0 MPa>= 1600 psiShear vs. Neoprene rubber. Substrate failure.; ASTM D1002
 >= 11.0 MPa>= 1600 psiShear vs. Nitrile rubber. Substrate failure.; ASTM D1002
 16.9 MPa2450 psiShear vs. Etched Aluminum; ASTM D1002
 22.4 MPa3250 psiShear vs. Grit Blasted Steel; ASTM D1002
 18.6 - 29.6 MPa2700 - 4300 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.250 min0.00417 hourFull cure 8 hours
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
BaseModified Ethyl
Color / appearanceclear
MIL A 46050Type II, Class II
SolventRemove Debonder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9069 / 233436

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.