MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Röchling Maywo® ABS/TPU
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Product characteristics:
  • Vacuum formable
  • Soft-touch effect
  • High scratch resistance
Product applications:
  • Trays
  • Automotive industry
  • Transportation industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³DIN EN ISO 1183-1
Water Absorption >= 0.30 %>= 0.30 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8080DIN EN ISO 2039-2
Hardness, Shore A 8383DIN EN ISO 868
Tensile Strength, Yield 32.0 MPa4640 psiDIN EN ISO 527
Elongation at Break 35 %35 %DIN EN ISO 527
Modulus of Elasticity 2.125 GPa308.2 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FDIN 53752
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 85.0 °C185 °Flong term
 100 °C212 °Fshort term
Vicat Softening Point 102 °C216 °FDIN EN ISO 306, Vicat B
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9198 / 232901

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.