MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QGel 920 High Refractive Index Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QGel 920 is a clear, very soft, tough, moderately cross-linked, silicone polymeric elastomer, offering exceptional clarity for optical transmission applications. This gel also provides self-healing protection to sensitive devices isolating them from shock, vibration and CTE stress. This particular silicone gel also provides excellent moisture protection and equally outstanding electrical properties over a broad temperature range.

Key Features:

  • One to one mix ratio
  • Soft, but resilient gel
  • Dispensing equipment not necessary
  • Good adhesion with QSil Primer #5

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccUncatalyzed A
 1.08 g/cc1.08 g/ccUncatalyzed B
Viscosity 1455 cP1455 cPUncatalyzed A
 1645 cP1645 cPUncatalyzed B
 
Mechanical PropertiesMetricEnglishComments
Penetration 5.0 - 9.0
@Temperature 150 °C,
Time 1800 sec
5.0 - 9.0
@Temperature 302 °F,
Time 0.500 hour
[mm], Cured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.485
@Temperature 49.0 °C
1.485
@Temperature 120 °F
 1.495
@Temperature 20.0 °C
1.495
@Temperature 68.0 °F
 1.50
@Temperature 14.0 °C
1.50
@Temperature 57.2 °F
 1.49
@Wavelength 589 nm
1.49
@Wavelength 589 nm
Transmission, Visible  89.95 %
@Wavelength 400 nm
89.95 %
@Wavelength 400 nm
 94 %
@Wavelength 600 nm
94 %
@Wavelength 600 nm
 94.5 %
@Wavelength 740 nm
94.5 %
@Wavelength 740 nm
 95 %
@Wavelength 700 nm
95 %
@Wavelength 700 nm
 96.9 %
@Wavelength 800 nm
96.9 %
@Wavelength 800 nm
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
 30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 60.0 min
@Temperature 100 °C
1.00 hour
@Temperature 212 °F
Gel Time 120 min120 minCatalyzed
 
Descriptive Properties
ColorTransparentUncatalyzed A
 TransparentUncatalyzed B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QGel 319 Optically Clear Silicone Gel
CHT Group QGel 323Y High Strength, Fast Curing Silicone Gel
CHT Group QGel 322Y General Purpose Silicone Gel
CHT Group QGel 322 General Purpose Silicone Gel
CHT Group QGel 321 Custom Silicone Gel

PACC2031 / 199419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.