MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Blockmix Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Vermiculite raw material base. Hydraulic bond. A 1000°C insulating castable with very low thermal conductivity and low density, mainly used as back up insulation. Conforms to ASTM Class N.

Applications: Designed for backup insulation up to 870°C as it contains Portland cement.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.465 g/cc0.0168 lb/in³dried to 110°C
Grain Size <= 3000 µm<= 3000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  0.600 MPa
@Treatment Temp. 1000 °C
87.0 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 1.00 MPa
@Treatment Temp. 815 °C
145 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 1.50 MPa
@Treatment Temp. 110 °C
218 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.140 W/m-K
@Temperature 600 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1000 °C<= 1830 °F
Shrinkage  0.00 - 0.20 %
@Treatment Temp. 110 °C
0.00 - 0.20 %
@Treatment Temp. 230 °F
 0.70 %
@Treatment Temp. 815 °C
0.70 %
@Treatment Temp. 1500 °F
 2.0 %
@Treatment Temp. 1000 °C
2.0 %
@Treatment Temp. 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 10 %10 %
CaO 37 %37 %
Fe2O3 4.0 %4.0 %
K2O+Na2O 3.0 %3.0 %Na2O + K2O
MgO 9.0 %9.0 %
SiO2 32 %32 %
TiO2 0.50 %0.50 %
 
Descriptive Properties
Net Material Required (kg/m³)420
Water Addition134-140% by weight, 20.1-21 L per bag, 15kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6395 / 203179

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.