MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Chockfast® PHILLYCLAD #8 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: PHILLYCLAD #8 is a two component fast setting epoxy laminating resin system designed for high strength fiberglass reinforced repairs to pipes, tanks, valves, and other equipment subject to corrosion or erosion. PHILLYCLAD #8 is also used to repair leaks in cargo heating coils, turbine drains, deck steam lines and other similar areas at operating temperatures to 220°C (428°F). PHILLYCLAD #8 has excellent resistance to salt water, crude and refined oil, gasoline, caustics and most acids. When used with four layers of fiberglass tape PHILLYCLAD #8 has the capability to withstand in excess of 70 kg/cm2 (1000 psi) hydrostatic pressure after one hour cure.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 220 °C428 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourGlass reinforced patches 3.0 to 6.5 mm thick.
Pot Life 10.0 - 15.0 min
@Temperature 22.2 °C
10.0 - 15.0 min
@Temperature 72.0 °F
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Colorblackhardener
 graymixed
 whiteresin
Mix Ratio by volume4 to 1Resin to hardener
Mix Ratio by weight4 to 1Resin to hardener
Viscosityliquid, brushable, pourable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9031 / 239541

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.