TABOREX TA 8030 LD contains the cross-linking catalyst and a stabilizer package. In addition it carries additives that protect the polymer from degradation caused by metal ions. Together with SILON´s Silane grafted TABOREX Compound this masterbatch completes a Sioplas System (PE-Xb) and provides processing and long term stability. Application: TABOREX TA 8030 LD is a catalyst Masterbatch according to the Sioplas System for the production of tubes and films in high temperature applications. TABOREX TA 8030 LD is specifically designed for the use in contact with metals or in composite systems. Information provided by Silon US LLC. |