MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Dow™ 2010 Ultra-Pure Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Dow 2010 Ultra-Pure Polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flexibility and environmental stress crack resistance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Oleamide Slip

Agency Ratings: DMF 1528; US FDA 21 CFR 177.1520©2.2

Form: Pellets

Processing Method: Injection Blow Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183
 0.922 g/cc0.0333 lb/in³ASTM D792
Melt Flow  1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 96.1 °C205 °FFreezing point; ASTM D3418
 96.1 °C205 °FFreezing point; ISO 3146
 109 °C228 °FPeak; ASTM D3418
 109 °C228 °FISO 3146
Vicat Softening Point 96.1 °C205 °FASTM D1525
 96.1 °C205 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF497 / 311190

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.