  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® OWF2 is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. Mylar® OWF2 has a thicker heat sealable layer than Mylar® OWF. This film is suitable for use in contact with food.

Approvals: FDA Food Contact Status - All gauges of Mylar® OWF2 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® OWF2 can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Thickness 15.2 microns0.600 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 100 %100 %ASTM D882A
Film Elongation at Break, TD 90 %90 %ASTM D882A
Coefficient of Friction, Dynamic 0.500.50A-B; ASTM D1894
Coefficient of Friction, Static 0.600.60ASTM D1894
Film Tensile Strength at Break, MD 172 MPa25000 psiASTM D882A
Film Tensile Strength at Break, TD 186 MPa27000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Maximum Service Temperature, Air 121 °C250 °F
Shrinkage, MD 1.25 %
@Temperature 150 °C,
Time 1800 sec
1.25 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.30 %
@Temperature 150 °C,
Time 1800 sec
0.30 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 3.5 %3.5 %ASTM D1003
Transmission, Visible 88.6 %88.6 %ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)5 cc/100 in2O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal)33000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge
DuPont Teijin Films Mylar® OWF Polyester Film, 48 Gauge

PDTZ9391 / 139711

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.