MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Magnesium Chloride, MgCl2 (Chloromagnesite)
Categories: Ceramic; Halide

Material Notes: White hexagonal leaflets, hygroscopic

Key Words: MgCl2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.325 g/cc0.08400 lb/in³
a Lattice Constant 3.632 Å3.632 Å
c Lattice Constant 17.795 Å17.795 Å
Formula Units/Cell (Z) 33
Molecular Weight 95.211 g/mol95.211 g/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000474-0.0000474cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 452.7 J/g194.8 BTU/lb
Melting Point 714 °C1320 °F
Boiling Point 1412 °C2574 °F
 
Descriptive Properties
CAS Number7786-30-3
ColorWhite
Crystal StructureRhombohedral

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Calcium Chloride, CaCl2
Potassium Chloride, KCl (Sylvite)
Mateck Potassium Chloride (KCl)
Lithium Carbonate, Li2CO3
Magnesium Chloride Hexahydrate, MgCl2-6H2O

EINOR0432 / 3561

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.