MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Tecnoflon® FOR TF Fluorelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: TECNOFLON® FOR TF is a high viscosity cure incorporated fluoroelastomer terpolymer (FKM) with 68% fluorine content. Tecnoflon® FOR TF is well suited for applications requiring better chemical resistance and/or long term heat resistance compared to fluoroelastomer copolymers.

Some of the basic properties of Tecnoflon® FOR TF are:
- Excellent chemical resistance
- Good compression set
- Excellent mold release
- Lack of mold fouling
- Superior mold flow

Tecnoflon® FOR TF can be used for compression and transfer molding of seals, gaskets or any item requiring excellent chemical resistance.
This material can be combined with the cure system and other typical fluoroelastomer compounding ingredients. Mixing can be accomplished with two-roll mills or internal mixers.
Tecnoflon® FOR TF can be extruded into hoses or profiles and can be calendered to make sheet stocks or belting. Finished goods can be produced by a variety of rubber processing methods.

Applications: Belts/Belt Repair; Blending; Gaskets; Hose; Profiles; Seals; Sheet

Features: Chemical Resistant; Good Flow; Good Mold Release; Good Processability; Heat Aging Resistant; High Viscosity; Low Compression Set; Terpolymer

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 57
@Temperature 121 °C
ML 1+10; ASTM D1646
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 68 %
 
Descriptive Properties
AdditiveProcessing Aid
AvailabilityEurope
 North America
ColorOff-White
FormsSlab
ProcessingCalendering; Compounding
 Compression Molding; Extrusion; Resin Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4514 / 280314

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.