System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® CI 31 F 000000 Copolyamide PA6/6I
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
Material Notes:
Copolyamide PA6/6I, low melt point (188-191°C), low viscosity, no additives, very high transparency, in compliance with FDA as far as the PA-layer is separated from the food by a 50 µm PE film
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.10
g/cc
ISO 1183
Water Absorption
10 %
Test Sim. to ISO 62
Moisture Absorption at Equilibrium
3.0 %
23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number
133
cm³/g
ISO 307, 1157, 1628
Melt Flow
28
g/10 min
@Load 5.00 kg,
Temperature 260 °C
Estimated using room temperature density; ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
80.0
MPa
ISO 527-1/-2
Elongation at Break
250 %
ISO 527-1/-2
Elongation at Yield
4.5 %
ISO 527-1/-2
Tensile Modulus
2400
MPa
ISO 527-1/-2
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
100
µm/m-°C
ISO 11359-1/-2
Melting Point
188
°C
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
54.0
°C
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
50.0
°C
ISO 75-1/-2
Descriptive Properties
Form
Pellets
ISO Short Name
ISO 1874: PA 6/ 6I,FNT,14-020
Processing
Film extrusion
Region
Asia Pacific
Europe
Near East/Africa
North America
South and Central America
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Mitsubishi Lemalloy® C61HL PPE-PA66 Alloy
Mitsubishi Lemalloy® BX528A-3 PPE-PA6 Alloy
Mitsubishi Lemalloy® BX503A-1 PPE-PA6 Alloy
Envalior Durethan® BKV 115 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Conditioned
PLANX0797 / 99012
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.