MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 6201 Styrene-Acrylic Resin
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Rovene® 6201 is an alkali soluble styrene-acrylic resin with a mid-range molecular weight supplied in a clear pellet form. Rovene® 6201 is a general use resin for overprint varnishes, water based inks and pigment dispersions. Rovene® 6201 provides excellent ink transfer and printability with high gloss.

Solution Preparation and Properties: The following are offered as starting point formulations. The resin should be cut under agitation and although Rovene® 6201 will dissolve at room temperature, the dissolution process can be greatly accelerated by the use of heat, up to 70°C.

Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6201 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.40 lb/gal
Volatiles <= 2.0 %
Molecular Weight 7000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 218[mgKOH/g]
 
Thermal PropertiesOriginal ValueComments
Softening Point 155 °C
Glass Transition Temp, Tg 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvabrite® S™ Lead-Free Solder
Lucas-Milhaupt Silvabrite® Lead-Free Solder
Lucas-Milhaupt Silvabrite® 100® Lead-Free Solder
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy

PMCP133 / 157410

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.