MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NYCOA 7551 Copolymer Nylon Alloy
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.

Information provided by NYCOA, Inc.

Key Words: PA 6, Polyamide 6, Nylon 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ASTM D792
Water Absorption 0.50 %0.50 %ASTM D570
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psiASTM D638
Elongation at Break 350 %350 %ASTM D638
Flexural Yield Strength 16.0 MPa2320 psiASTM D790
Flexural Modulus 0.400 GPa58.0 ksiASTM D790
Izod Impact, Notched 6.50 J/cm12.2 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °FASTM D789
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 °C482 °F
Rear Barrel Temperature 200 °C392 °F
Middle Barrel Temperature 230 °C446 °F
Front Barrel Temperature 250 °C482 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 76.0 °C169 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NYCOA 2012 Copolymer Nylon
NYCOA 2011 Copolymer Nylon
NYCOA 2001 PA 6
NYCOA 1838 Copolymer Nylon Alloy
Envalior Arnitel® VT3104 TPC-ET, Extrusion Grade

PNYCOA24 / 55570

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.