MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Nymax™ 1213 HS Black 125 Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Molded Test Bars: Dry as Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Water Absorption 1.5 %
@Thickness 0.508 mm,
Time 86400 sec
1.5 %
@Thickness 0.0200 in,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 79.3 MPa11500 psiType I, 5.1 mm/min; ASTM D638
Elongation at Yield 20 %20 %Type I, 5.1 mm/min; ASTM D638
Flexural Modulus 2.86 GPa415 ksiASTM D790
Izod Impact, Notched 0.427 J/cm
@Thickness 1.57 mm,
Temperature -40.0 °C
0.800 ft-lb/in
@Thickness 0.0618 in,
Temperature -40.0 °F
Across Flow, Compression Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
@Thickness 3.18 mm
149 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Descriptive Properties
AdditiveHeat Stabilizer
AppearanceBlack
FeaturesHeat Stabilized
FormsPellets
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityNorth America
 South America
UsesIndustrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Avient Versaflex™ CL2003X Thermoplastic Elastomer (TPE)
Avient Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66)

PH1PN9263 / 103099

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.