Product Description: PA 6, 15% Glass Fiber Reinforced, 25% Mineral Reinforced, Heat Stabilized, Lubricated, UV-stabilized for Automotive Exterior Applications, Natural Color Availability: North America Filler/Reinforcement: Glass Fiber, 15% Filler by Weight; Mineral, 25% Filler by Weight Additive: Heat Stabilizer; Lubricant; UV Stabilizer Features: Heat Stabilized; Lubricated; UV Stabilized Uses: Automotive Applications RoSH Compliance: RoSH Compliant Appearance: Natural Color Information provided by Ravago Manufacturing Americas |