MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

PolyMirae Moplen HP480S Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen HP480S is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP480S is a homopolymer selected by customers for use in injection molding of DVD case, housewares containers, closures and toys. Moplen HP480S resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features: Easy processing/Good dimensional stability/ Good impact and stiffness balance/Good surface finish

Typical Applications: CD, DVD cases/Housewares containers/Closures/Toys

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.3 MPa4980 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus 1.47 GPa213 ksiASTM D790
Izod Impact, Notched 0.196 J/cm
@Temperature 23.0 °C
0.367 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen RP344N Injection Molding Grade Polypropylene
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene
PolyMirae Moplen RP348S Injection Molding Grade Polypropylene
PolyMirae Moplen RP348SK Injection Molding Grade Polypropylene
Total PPH 12020 Polypropylene Homopolymer, Injection Molding

PMIRAF40 / 183261

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.