MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 6003-75A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Categories: Polymer; Thermoplastic; Elastomer, TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 757510 s delay; ASTM D 2240
Tensile Strength at Break 8.76 MPa1270 psiDie C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tensile Strength, Yield 3.17 MPa460 psiDie C 0.125 in (3.2 mm); 20 in/min (500 mm/min); 100%; ASTM D 412
Elongation at Break >= 500 %>= 500 %Die C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tear Strength 50.0 kN/m285 pliDie C; ASTM D 624
Peel Strength >= 6.14 kN/m>= 35.0 pliPC/PBT; 90 degrees, 20 in/min (500 mm/min); ISO 813
 >= 6.14 kN/m>= 35.0 pliPC/PMMA; 90 degrees, 20 in/min (500 mm/min); ISO 813
Compression Set  23 %
@Temperature 23.0 °C,
Time 79200 sec
23 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 65 %
@Temperature 70.0 °C,
Time 79200 sec
65 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 238 °C380 - 460 °F
Mold Temperature 21.1 - 48.9 °C70.0 - 120 °F
Drying Temperature 76.7 °C
@Time 7200 - 14400 sec
170 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer
RTP Company RTP 6003-55A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
RTP Company RTP 132 UV  Polypropylene (PP) Talc 30% - UV Stable
RTP Company RTP 6003-45A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
RTP Company RTP 1500-30D Polyether-Ester Block Copolymer (TEEE / COPE)

PQZUA21301 / 134776

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.