MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics TAIRILOY® AC2190 PC + ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Product Description: Extrusion Grade. Characteristics: Extrusion molding; High impact.
Availability: Asia Pacific; Europe; North America
Features: High Impact Resistance
Agency Rating: EC 1907/2006 (REACH)
UL File Number: E162823
Processing Method: Extrusion

Information provided by Formosa Chemicals & Fiber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 240 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 464 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength 66.0 MPa9570 psiASTM D638
Flexural Strength 88.3 MPa12800 psiASTM D790
Flexural Modulus 2.05 GPa298 ksiASTM D790
Izod Impact, Unnotched 8.01 J/cm
@Thickness 3.17 mm
15.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 6.35 mm
259 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Flammability, UL94  HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
All Color
 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
All Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCPD053 / 268167

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.