MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total LF 38 YS CF MDPE, pipe
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: FINATHENE® LF 38 YS CF is a cadmium-free yellow stripe compound designed to be used in combination with FINATHENE® 3802 B for gas pipe application.

The base polymer of FINATHENE® LF 38 YS CF is the same as the base polymer of FINATHENE® 3802 B.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oxidative Induction Time (OIT) >= 30 min>= 30 min200°C; EN 728
Melt Flow 0.90 g/10 min
@Load 5.00 kg
0.90 g/10 min
@Load 11.0 lb
ISO 1133

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
LyondellBasell Lupolen 5261 Z Q 456 High Density Polyethylene, Pipe and Sheet Extrusion Grade
Total 3802 B HDPE, cable, sheet, pipe, injection molding
Total HP 401 MDPE, pipe, cable, sheet

PFINAP121 / 38704

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.