MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process. HexFlow® RTM 6 is a premixed epoxy system for service temperatures from -60°C up to 180°C (-75°F up to 350°F). At room temperature, it is a brown translucid paste but its viscosity decreases quickly by increasing the resin temperature.

Advantages: Monocomponent system; Already degassed; High glass transition temperature; Excellent hot/wet properties; Easy to process (low injection pressure); Long injection window = 150 min at recommended injection temperature; Low moisture absorption; Short, simple cure cycles.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
@Temperature 25.0 °C
Uncured
 1.14 g/cc
@Temperature 25.0 °C
Cured
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 75.0 MPaNeat Resin; ASTM D638
 860 MPaTensile Warp, Dry/RT; Pr EN 2597 B
 830 MPa
@Temperature 80.0 °C
Tensile Warp, Wet; Pr EN 2597 B
Elongation at Break 3.4 %Neat Resin; ASTM D638
Tensile Modulus 2.89 GPaNeat Resin; ASTM D638
 63.0 GPaTensile Warp, Dry/RT; Pr EN 2597 B
 63.0 GPaTensile Warp, Wet; Pr EN 2597 B
Flexural Yield Strength 132 MPaNeat Resin; ASTM D790
Flexural Modulus 3.30 GPaNeat Resin; ASTM D790
Compressive Yield Strength 700 MPaCompression Warp, Dry/RT; Pr EN 2856 TA
 536 MPa
@Temperature 80.0 °C
Compression Warp, Wet; Pr EN 2856 TA
Compressive Modulus 60.0 GPaCompression Warp, Dry/RT; Pr EN 2856 TA
 63.0 GPa
@Temperature 80.0 °C
Compression Warp, Wet; Pr EN 2856 TA
Shear Modulus 4.30 GPaIn-Plane Shear, Dry/RT; AiTM 1.0002
 35.0 GPa
@Temperature 80.0 °C
In-Plane Shear, Wet; AiTM 1.0002
Shear Strength 67.0 MPaI.L.S. Warp, Dry/RT; Pr EN 2563
 100 MPaIn-Plane Shear, Dry/RT; AiTM 1.0002
 78.0 MPa
@Temperature 80.0 °C
In-Plane Shear, Wet; AiTM 1.0002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Gel Time 5.00 min
@Temperature 240 °C
 12.0 min
@Temperature 210 °C
 30.0 min
@Temperature 180 °C
 95.0 min
@Temperature 140 °C
 >= 240 min
@Temperature 120 °C
Shelf Life 9.00 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Alloy Steel
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler

PHEXC482 / 99301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.