MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Therm-O-Stix Fibrous Adhesive
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Therm-O-Stix is a fibrous adhesive material composed of sodium silicate and cellulose fiber, and contains no asbestos fibers. Therm-O-Stix is a fast setting compound used for bonding board or blanket insulation to surfaces and has excellent adherence for holding in place while other refractories are being installed. It can be used to waterproof board and blanket insulation to prevent the insulation from absorbing moisture from product being installed, such as castable and moldable refractories. Therm-O-Stix can be brushed or troweled on the products for bonding to various surfaces.

When coating material to make impervious to moisture, coverage will be approximately 20 sq. ft. per gallon. When spot troweling to stick board or blankets to surfaces, coverage will be approximately 25 sq. ft. per gallon.

Features:

  • Finishing cement recommended for temperatures up to 1400°F
  • Finishing cement provides a strong protective coating for other insulation materials
  • Insulating cement recommended for temperatures up to 1800°F
  • Insulating cement is a non-corrosive cement with outstanding adhesion
  • Fibrous adhesive maximum service temperature 1200°F
  • No asbestos fibers
  • Fast setting compound
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.240 g/cc0.00867 lb/in³dry
     1.314 g/cc0.04747 lb/in³wet
    Ash 3.0 %3.0 %
     
    Thermal PropertiesMetricEnglishComments
    Maximum Service Temperature, Air 649 °C1200 °F
     
    Component Elements PropertiesMetricEnglishComments
    Alkalis 23 %23 %
    SiO2 74 %74 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Overview of materials for Methacrylate Adhesive
    Overview of materials for Epoxy Adhesive
    Momentive Performance Materials RTV6809 Aluminum Adhesive Sealant, Industrial Plastic Adhesive
    Momentive Performance Materials RTV109 Aluminum Adhesive Sealant, High Strength Paste
    Lord Adhesives 7610DTM Direct-to-metal Adhesive/Sealant

    CTHERM257 / 2577

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.