MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® LED sign grade (Resist SG) Acrylic thermoplastic sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: ACRYLITE® LED sign grade: ACRYLITE® LED sign grade (formerly Resist SG) is a continuously manufactured, thermoplastic sheet product developed specifically for the sign market. It is produced utilizing innovative polymers and the same proprietary technology used when manufacturing ACRYLITE® extruded sheet. ACRYLITE® LED sign grade is the universal sign product which combines light weight and high optical quality with outstanding ease of fabrication and greater impact strength than standard acrylic sheet.

Characteristics: ACRYLITE® LED sign grade is a versatile thermoplastic sheet that is rigid, tough, lightweight, and offers ease of fabrication and machining. Cutting, routing, drilling, forming and cementing can be performed on ACRYLITE® LED sign grade. Specifically designed for the sign industry, ACRYLITE® LED sign grade is ideal for use in channel letters, formed letters and shapes as well as back painted signs. ACRYLITE® LED sign grade offers the look of acrylic with the impact strength required for fabrication, handling, shipping and sign installation.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D729
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
Tensile Strength at Break 61.4 MPaASTM D638
Elongation at Yield 4.8 %ASTM D638
Tensile Modulus 2410 MPaASTM D638
Flexural Strength 96.5 MPaASTM D790
Flexural Modulus 2.28 GPaASTM D790
Izod Impact, Notched (ISO) 0.630 kJ/m²ASTM D256
Gardner Impact 20.0 in-lbASTM D5420
Dart Drop, Total Energy 4.60 ft-lbASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 71.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °CASTM D648
Vicat Softening Point 106 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Gloss 125 %20°; ASTM D523
Transmission, Visible 90 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4BR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk5BR Impact Acrylic Polymer

PEVONIL077 / 196281

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.