MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Taro Plast Taromid A 280 G4 X0 Nylon 66, 20% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Polyamide 66 medium viscosity, 20% glass fibers reinforced, flame retardant UL94 V0. Available: all colors, heat stabilized (H), release agent (W).

Information provided by Taro Plast S.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 - 1.42 g/ccISO 1183
Filler Content 20 %ISO 3451
Water Absorption 0.75 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 5.5 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527
Elongation at Break 3.5 %ISO 527
Tensile Modulus 7600 MPaISO 527
Flexural Strength 125 MPaISO 178
Flexural Modulus 7000 MPaISO 178
Izod Impact, Notched 50.0 J/m127x12.7x3.2; ASTM D256
Charpy Impact, Notched 4.00 kJ/m²80x10x4; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Comparative Tracking Index 325 VMethod A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°CISO 11359
Maximum Service Temperature, Air 90.0 °C
@Time 468000 sec
IEC 60216
Hot Ball Pressure Test 205 °CIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °CISO 75/A
Vicat Softening Point 240 °C
@Load 1.00 kg
ISO 306
Flammability, UL94 V-0
@Thickness 0.880 mm
127x2.17xThickness
Oxygen Index 32 %6.3x12.7x3.2; ASTM D2863
Glow Wire Ignition Temperature 850 °C
@Thickness 1.00 mm
60x60xThickness; IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
60x60xThickness; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTARO016 / 283124

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.