MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay MR Film Fluoropolymer Film
Categories: Polymer; Film; Thermoset; Fluoropolymer, TS

Material Notes: Description: Release film. Ideally suited to aerospace applications.

Features & Benefits:

  • High performance fluoropolymer based film
  • High elongation and excellent yield under stress ensure a superior surface finish on the cured laminate
  • Maintains high performance even when used in ultra-high temperature conditions
  • Release well (and resists break down) from even the most aggressive resin systems, including epoxy, BMI and polyimide
  • Available in a range of perforation patterns.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.14 g/cc
Thickness 25.0 microns
 50.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4300 psi
Elongation at Break 400 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 315 °C
 
Descriptive Properties
ColorRed, beige and blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay FM® 10 Epoxy Syntactic Core
Solvay CYCOM® 985 Epoxy Neat Resin
Overview of materials for Epoxy, Cast, Unreinforced
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets

PCYTED274 / 180576

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.