MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Röchling Durostone® UPM S13 LST Reinforced Polyester Sheet
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Durostone® UPM S13 LST is a fiber-reinforced plastic with an exceptionally good behavior in fire. The flammability of plastics attains a particular value of FVO /> 1mm. It has a low toxicity and low smoke density. Durostone® UPM S13 LST meets requirement R11, hazard level HL3, for arc resistant insulation materials of EN 45545-2:2013.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.10 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 80.0 MPaParallel; ISO 527
Modulus of Elasticity 16.0 GPaPerpendicular; ISO 178
Flexural Strength 160 MPaPerpendicular; ISO 178
Compressive Strength 250 MPaPerpendicular; ISO 604
Izod Impact, Notched (ISO) 100 kJ/m²Parallel; ISO 179
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 - 30.0 µm/m-°C
Thermal Conductivity 0.300 W/m-KISO 8302
Flammability, UL94 V-0
@Thickness >=5.00 mm
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9075 / 232778

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.