MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Special Metals INCONEL® Alloy C-276
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures. Used in pollution control, chemical processing, pulp and paper production, and waste treatment. Standard product forms are round, forging stock, tube, pipe, plate, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: ASME SB-574, SB-575, SB-619, SB-622, SB-626, Boiler Code Sections I, III, VIII, IX; Werkstoff Nr. 2.4819, Nickel-Chromium Alloy; UNS N10276; ASTM B 574, B 575, B 619, B 622, B 626, B 751; NACE MR-01-75; DIN 17744, 17750-17752, C276
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 790 MPaAnnealed
 620 MPa
@Temperature 550 °C
Annealed prior to test
Tensile Strength, Yield 415 MPaAnnealed
 230 MPa
@Temperature 550 °C
Annealed prior to test
Elongation at Break 62 %Annealed prior to test.
 60 %
@Temperature 550 °C
Annealed prior to test.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0001229 ohm-cm
Magnetic Permeability 1.0002at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.2 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.427 J/g-°C
Thermal Conductivity 9.80 W/m-K
Melting Point 1325 - 1370 °C
Solidus 1325 °C
Liquidus 1370 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.010 %
Chromium, Cr 14.5 - 16.5 %
Cobalt, Co <= 2.5 %
Iron, Fe 4.0 - 7.0 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 15 - 17 %
Nickel, Ni 55 %As remainder
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.080 %
Sulfur, S <= 0.030 %
Tungsten, W 3.0 - 4.5 %
Vanadium, V <= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Special Metals INCONEL® Alloy 718
Special Metals INCONEL® Alloy 625
Special Metals INCONEL® Alloy 617
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276

NINC51 / 17408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.