MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Meehanite GC-40 Flake Graphite Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake drums and pressure castings up to 2 1/2" thick.

General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.

Information provided by Meehanite Marketing Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.25 g/cc7.25 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 190190Nominal
Tensile Strength, Ultimate 276 MPa40000 psi
Tensile Strength, Yield 100 MPa14500 psi.01% permanent set
Modulus of Elasticity 114 GPa16500 ksi
Modulus of Rupture 0.552 GPa80.0 ksi
Compressive Strength 1030 MPa150000 psi
Poissons Ratio 0.300.30
Fatigue Strength 121 MPa17500 psi
Machinability 47 %47 %Dalcher
Shear Modulus 50.0 GPa7250 ksi
Shear Strength 276 MPa40000 psi
Izod Impact Unnotched 16.3 - 27.1 J
@Diameter 20.3 mm
12.0 - 20.0 ft-lb
@Diameter 0.798 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.9 µm/m-°C
@Temperature 37.8 - 538 °C
6.60 µin/in-°F
@Temperature 100 - 1000 °F
Thermal Conductivity 46.8 W/m-K
@Temperature 10.0 - 232 °C
325 BTU-in/hr-ft²-°F
@Temperature 50.0 - 450 °F
Shrinkage 1.0 - 1.3 %1.0 - 1.3 %Patternmaker Shrinkage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gray Cast Iron, ASTM A 48 Class 40
Meehanite GA-50 Flake Graphite Cast Iron
Overview of materials for Gray Cast Iron
Meehanite GF-20 Flake Graphite Cast Iron
United Cast Bar Unibar 200 Continuously Cast Iron

NMEE03 / 18224

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.