MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Polifor® C40 CAMU/40 Sound Dead Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D1505
Linear Mold Shrinkage 0.0080 - 0.0090 cm/cmASTM D955
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 20.0 MPaASTM D638
Elongation at Break 15 %ASTM D638
Flexural Modulus 2500 MPaASTM D790
Izod Impact, Notched 30.0 J/mASTM D256/A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 70.0 °C50°C/h at 50 N; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 230 °CCylinder Temperature
Mold Temperature 40.0 - 60.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 4820WZ Polypropylene, Impact Copolymer
SCG Chemicals EL-Pro™ P842J Polypropylene Injection Molding
Total PPC 4944CWZ Polypropylene, Impact Copolymer
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat

PSOFS810 / 162274

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.