Description: ACC15 is a low viscosity, 1-component, condensation curing silicone coating. The uncured product can be applied by pouring or brushing and is readily cured to a tough, transparent rubber. It can be used to coat printed circuit boards to prevent ingress of water and environmental contaminants. Key Features - UL listed file number E493561
- Room temperature cure or mild heat acceleration at 60ºC
- Low viscosity
- 100% solids
- Fluorescent UV aid for production QA checks
- Excellent adhesion to many substrates
- Low odour
- RoHS compliant
Application: The bulk product may be poured or brushed onto the circuit. Pouring or brushing will give a film thickness of 100 to 1000 microns. The product contains an UV trace to allow inspection of the board after coating to ensure complete and even coverage. Boards should be thoroughly cleaned before coating for best adhesion / performance. Coating over no clean fluxes is possible so long as other surface contaminants are not present.Cured Elastomer: After 7 days at 25°C / 55 +/- 5% Humidity on a 3 mm thick test sheet. Information provided by CHT Group |