MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 are consumer durables and 35, 65, and 95-gallon refuse carts.

Regulatory Status: Alathon M4855 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Specific recommendations for processing M4855 can only be made when the processing conditions, equipment and end use application are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.593 - 0.625 g/ccASTM D1895
Density 0.948 g/ccASTM D1505
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 8.00 inEquistar test
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3500 psi50 mm/min; ASTM D638
Tensile Strength, Yield 3480 psi50 mm/min; ASTM D638
Elongation at Break 1490 %50 mm/min; ASTM D638
Elongation at Yield 12 %50 mm/min; ASTM D638
Tensile Modulus 92200 psi1% Secant; 50mm/min; ASTM D638
 117000 psi50mm/min; ASTM D638
Flexural Modulus 146000 psi12.5 mm/min; ASTM D790
 112000 psi
@Strain 2 %
Secant; 12.5 mm/min; ASTM D790
Flexural Modulus, 1% Secant 138400 psi2.5 mm/min; ASTM D790
Izod Impact, Notched 1.10 ft-lb/inASTM D256
 NB
@Temperature -18.0 °C
ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Melting Point 262.2 °FASTM D3418
Crystallization Temperature 113.1 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 64.0 °CASTM D648
Vicat Softening Point 125 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 °F
Middle Barrel Temperature 470 °F
Front Barrel Temperature 475 °F
Nozzle Temperature 475 °F
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DMDA-8904 NT 7 High Density Polyethylene Resin
Dow DMDA-8907 NT 7 High Density Polyethylene Resin
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Chevron Phillips Marlex® C513UV High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin

PEQU0791 / 104147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.