MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ganpati Exim EPDM 6305
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: EPDM 6305/7505 is a high Mooney, high ethylene content, fast curing EPDM rubber characterized by high green strength and intended for use in areas requiring excellent mechanical properties and good extrusion performance. Typical fields of application include (but are not limited to ) production of automotive parts, electrical appliances, cables and waterproofing membranes. EPDM 6305/7505 permits a high level of filler.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 45 - 54
@Temperature 125 °C
ML 1+4
 55 - 64
@Temperature 125 °C
ML 1+4
 65 - 75
@Temperature 125 °C
ML 1+4
 76 - 85
@Temperature 125 °C
ML 1+4
Ash <= 0.20 %
 
Descriptive Properties
Content<0.008%Vanadium
 <0.15%Stabilizer
 24-30%Propylene chains
 4.3-5.7%ENB mass
Mass losses at drying<0.7%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI062 / 317346

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.