Vydyne 21SPF1 is a general-purpose, unfilled, lubricated PA66 resin with an enhanced crystallization temperature, and enhanced processing. Designed principally to further decrease cycle time, with a for injection-molding fabrication, this product offers a combination of engineering properties characterized by high strength; rigidity; good toughness; high melt point; good surface lubricity; abrasion resistance; and resistance to many chemicals, machine and motor oils, solvents and gasoline.Information provided by Ascend Performance Materials. |