MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parker Chomerics CHO-SEAL 1298 EMI Shielding Material
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in corrosion resistance over products previously available. In fact, a virtually corrosion-proof EMI flange system is obtained when CHO-SEAL 1298 gaskets are used in conjunction with Chomerics CHO-SHIELD® 2000 series corrosion resistant coatings on aluminum flanges.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 - 2.25 g/cc1.75 - 2.25 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 63 - 7763 - 77ASTM D2240
Tensile Strength at Break >= 1.24 MPa>= 180 psiASTM D412
Elongation at Break 60 - 260 %60 - 260 %ASTM D412
Tear Strength 6.13 kN/m35.0 pliASTM D624
Compression Set <= 30 %
@Temperature 100 °C,
Time 252000 sec
<= 30 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.012 ohm-cm<= 0.012 ohm-cmMIL-DTL-83528
 <= 0.015 ohm-cm<= 0.015 ohm-cmLife Test/Post Tensile; MIL-DTL-83528 Para.4.6.12
Shielding Effectiveness  >= 55 dB
@Frequency 200000 Hz
>= 55 dB
@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
 >= 75 dB
@Frequency 4.00e+10 Hz
>= 75 dB
@Frequency 4.00e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 90 dB
@Frequency 1e+10 Hz
>= 90 dB
@Frequency 1e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 95 dB
@Frequency 2.00e+9 Hz
>= 95 dB
@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 100 dB
@Frequency 5.00e+8 Hz
>= 100 dB
@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 >= 110 dB
@Frequency 1e+8 Hz
>= 110 dB
@Frequency 1e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.20 W/m-K
@Pressure 2.07 MPa
8.33 BTU-in/hr-ft²-°F
@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °FFlex TR10; ASTM D1329
 
Descriptive Properties
BinderFluorosilicone
EMP Survivability >0.9 kA / inMIL-DTL-83528 Para.4.6.16
FillerPassivated Ag/Al
Gravimetric Weight Loss, mg3.5
Heat Aging <0.015 ohm-cmMIL-DTL-83528 Para.4.6.15
Type DMIL-DTL-83528
Vibration Resistance, After<0.012 ohm-cmMIL-DTL-83528 Para.4.6.13
Vibration Resistance, During, ohm-cm max<0.015 ohm-cmMIL-DTL-83528 Para.4.6.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer
Parkway Products Thixomolded® AZ91D Magnesium
Aluminum A360.0-F Die Casting Alloy
ATG s.r.l. FVMQ Fluorosilicone Rubber

PCHOME129 / 28351

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.