System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ASA Polymer
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
PBT + ASA Blend, Glass Fiber Reinforced
Material Notes:
PBT+ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish
The Pocan® product line was transferred to Envalior, but this product was discontinued prior to that transaction.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.433
g/cc
ISO 1183
Water Absorption
0.40 %
Test Sim. to ISO 62
Moisture Absorption at Equilibrium
0.10 %
23°C/50% R.H.; Test Sim. to ISO 62
Linear Mold Shrinkage, Flow
0.0040
cm/cm
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
ISO 294-4, 2577
Melt Flow
37
g/10 min
@Load 2.16 kg,
Temperature 270 °C
Estimated using room temperature density; ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
110
MPa
ISO 527-1/-2
Elongation at Break
2.5 %
ISO 527-1/-2
Tensile Modulus
7500
MPa
ISO 527-1/-2
Charpy Impact Unnotched
45.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
50.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Puncture Energy
2.20
J
ISO 6603-2
Electrical Properties
Original Value
Comments
Comparative Tracking Index
200
V
IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
30.0
µm/m-°C
ISO 11359-1/-2
CTE, linear, Transverse to Flow
100
µm/m-°C
ISO 11359-1/-2
Melting Point
225
-
260
°C
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
175
°C
ISO 75-1/-2
Deflection Temperature at 8.0 MPa
120
°C
ISO 75-1/-2
Flammability, UL94
HB
@Thickness 0.800 mm
IEC 60695-11-10
HB
@Thickness 1.60 mm
IEC 60695-11-10
Processing Properties
Original Value
Comments
Melt Temperature
270
°C
Injection Molding; ISO 294
Mold Temperature
90.0
°C
Injection Molding; ISO 10724
Descriptive Properties
Additives
Release agent
Form
Pellets
ISO Short Name
ISO 7792-1-PBT+PET+ASA,GHMR,07-080,GF20
Processing
Injection molding
Region
Asia Pacific
Europe
Near East/Africa
North America
South and Central America
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Techmer ES HiFill® ASA GF20 20% Glass Filled
INEOS Styrolution Luran® S KR2858 G3 Acrylonitrile Styrene Acrylate (ASA)
INEOS Styrolution Luran® S KR 2859 UV ASA
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid
PLANX0922 / 99137
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.