MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® HTNFE8200 NC010 PA6T/XT-HI
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Unreinforced, Toughened, PPA, High Performance Polyamide

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccDAM; ISO 1183
Melt Density 0.970 g/cc
@Temperature 325 °C
Water Absorption 6.3 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.90 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 68.0 MPa50% RH; ISO 527-1/-2
 68.0 MPaDAM; ISO 527-1/-2
Elongation at Break 10 %Nominal; 50% RH; ISO 527-1/-2
 14 %Nominal; DAM; ISO 527-1/-2
Elongation at Yield 4.4 %50% RH; ISO 527-1/-2
 5.5 %DAM; ISO 527-1/-2
Tensile Modulus 2200 MPaDAM; ISO 527-1/-2
 2300 MPa50% RH; ISO 527-1/-2
Flexural Modulus 2100 MPaDAM; ISO 178
 2200 MPa50% RH; ISO 178
Poissons Ratio 0.3950% RH
 0.39DAM
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 75.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 75.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance >= 1.00e+15 ohm50% RH; IEC 62631-3-2
Comparative Tracking Index 600 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°CDAM; ISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 91.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 84.0 µm/m-°CDAM; ISO 11359-1/-2
 72.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 86.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Specific Heat Capacity 2.22 J/g-°C
@Temperature 325 °C
Melt
Thermal Conductivity 0.180 W/m-K
@Temperature 325 °C
Melt
Melting Point 300 °C10°C/min; DAM; ISO 11357-1/-3
 300 °Cfirst heat; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 138 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 126 °CDAM; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.750 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 325 °COptimum, Injection
 320 - 330 °CRange, Injection
Mold Temperature 80.0 - 120 °CInjection
Ejection Temperature 225 °CInjection
Drying Temperature 100 °CInjection
Dry Time 6.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6T/XT-I,,M1G1HNR,S10-020
Part Marking Code>PA6T/XT-HI<ISO 11469
 >PPA-I<SAE J1344
PolymerPA6T/XT-I
Resin IdentificationPA6T/XT-HIISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether
Celanese Zytel® HTN51G45HSL NC010 PA6T/XT-GF45
Celanese Zytel® HTN51G15HSL BK083 PA6T/XT-GF15
Celanese Zytel® HTN51G15HSL NC010 PA6T/XT-GF15
Celanese Zytel® HTN51G35EF BK083 PA6T/XT-GF35

PDSX5458 / 198098

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.