Standard, high flow, fast molding cycle grade. DURACON® POM is mainly used in applications centered on mechanical components such as gears, screws, and bearings, and in important parts requiring chemical and heat resistance. Key properties: sliding ability, fuel resistance/oil resistance, low VOC, food related applications, chemical resistance, creep resistance, dimensional stability, fatigue resistance, low friction/low wear, suitability for insert / outsert molding. Information provided by Polyplastics |