MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions 120 Series 124A Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® 124A is low molecular weight resin providing lower gelation and faster fusion characteristics. It provideds good chemical foamability for producing medium to high density foams. It gives good dispersability for plastisol formulations. Geon® 124A is recommended for medium to high density foam applications where good physical properties at lower temperatures are required.

Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 124A, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390 (formulation): 100phr Geon® 124A, and 60phr DOP

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Bulk Density 0.465 g/cc0.0168 lb/in³
Fineness 4.754.75Hegman, North Fineness; Geon® 390
Relative Viscosity 2.12 cP2.12 cPCorrelation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 4.95 cP4.95 cPInitial Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 5.43 cP5.43 cPInitial Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 6.15 cP6.15 cPOne Day Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
 6.93 cP6.93 cPOne Day Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation); Internal Method
Viscosity Measurement 0.850.85Inherent; ASTM D1243-60-A
Melt Flow 132 g/10 min
@Pressure 0.655 MPa
132 g/10 min
@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 17.7 MPa2570 psiOptimum; With provided formulation; ASTM D638
 
Optical PropertiesMetricEnglishComments
Gloss 92 %92 %60 Degree Fused 5 mins @ 350 F Geon® ALTC 65 (with provided formulation); Internal Method
Transmission, Visible 75 %75 %Geon® ALTC 66 (with provided formulation); Internal Method
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.060 %0.060 %Karl FisherGeon® STP 683; Internal Method
 
Descriptive Properties
FeaturesFoamable
 Low Molecular Weight
FormsPowderFine, White Powder
Gel Temperature69 °CInternal Method; Geon® ALTC 29 (with provided formulation)
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value64Internal Method; Correlation, 0.5gm/ 100ml
Methanol Extractables3.2%Internal Method; Geon® STP 894
Polymerization ProcessMicrosuspension
Processing MethodCoating
 Dip Coating
 Rotational Molding
 Slush Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Vinyl Chloride Monomer< 9 ppmInternal Method; Geon® STP 1005
UsesCoating Applications
 Foam

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 120 Series 121A Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Inovyn 561SF Vinyl Chloride - Vinyl Acetate copolymer Paste - filler
Inovyn 373ND Polyvinyl Chloride Low Viscosity Paste

PH0POL0860 / 145429

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.