MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Polytek Poly LiteCast Rigid & Flexible Polyurethane Casting Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: Poly LiteCast and Poly Plasti-Flex Liquid Plastics are used to produce decorative moldings, tools, models, patterns, fixtures, duplicate masters and more. Use Poly LiteCast Liquid Plastic when a rigid plastic with a wood-like density is required. Use Poly Plasti- Flex to produce slightly flexible parts such as decorative trim molding, props, special effects castings, and impact-resistant items.

Product Line Features:

  • Safe and easy to machine (contains no silica)
  • Reproduces fine detail
  • Create rigid castings with a wood-like density

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.780 g/cc
Viscosity 2480 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
Tensile Strength 2398 psi
Elongation at Break 3.0 %
Modulus of Elasticity 105.4 ksi
Flexural Strength 4402 psi
@Strain 5.0 %
Flexural Modulus 16630 psi
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 4.00 hourDemold Time
Pot Life 5.00 min
 
Descriptive Properties
Cured ColorTan
Maximum Exotherm251°F
Mix Ratio By Weight1A:1B
Specific Volume35 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTK5088 / 251080

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.