Carbon Fiber 35% - PTFE 15% - High Flow Comments: - Carbon Fiber
- PTFE Lubricated
- High Flow
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |