MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

EOS Titanium Ti64 ELI DMSL on EOS M 290
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Description: EOS Titanium Ti64ELI has a chemical composition and corresponding to ASTM F136 and ASTM F3001. Ti64ELI is well-known light alloy, characterized by having excellent mechanical properties and corrosion resistance combined with low specific weight and biocompatibility. This material is ideal for many high-performance applications. Parts built with EOS Titanium Ti64ELI powder can be machined, shot-peened and polished in as-built and heat treated states. Due to the layerwise building method, the parts have a certain an-isotropy.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.41 g/cc0.159 lb/in³ISO 3369
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 320
@Load 5.00 kg
320
@Load 11.0 lb
EN ISO 6507-1
Tensile Strength, Ultimate  1055 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
153000 psi
@Treatment Temp. 1470 °F,
Time 2.00 hour
Horizontal, Heat treated; ISO 6892-1
 1075 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
155900 psi
@Treatment Temp. 1470 °F,
Time 2.00 hour
Vertical, Heat treated; ISO 6892-1
Tensile Strength, Yield  945 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
137000 psi
@Treatment Temp. 1470 °F,
Time 2.00 hour
Horizontal, Heat treated; ISO 6892-1
 965 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
140000 psi
@Treatment Temp. 1470 °F,
Time 2.00 hour
Vertical, Heat treated; ISO 6892-1
Elongation at Break  13 %
@Treatment Temp. 800 °C,
Time 7200 sec
13 %
@Treatment Temp. 1470 °F,
Time 2.00 hour
Horizontal, Heat treated; ISO 6892-1
 14 %
@Treatment Temp. 800 °C,
Time 7200 sec
14 %
@Treatment Temp. 1470 °F,
Time 2.00 hour
Vertical, Heat treated; ISO 6892-1
Reduction of Area  >= 25 %
@Treatment Temp. 800 °C,
Time 7200 sec
>= 25 %
@Treatment Temp. 1470 °F,
Time 2.00 hour
Horizontal; ISO 6892-1
 >= 25 %
@Treatment Temp. 800 °C,
Time 7200 sec
>= 25 %
@Treatment Temp. 1470 °F,
Time 2.00 hour
Vertical; ISO 6892-1
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 6.5 %5.5 - 6.5 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.25 %<= 0.25 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.13 %<= 0.13 %
Titanium, Ti 87.97 - 91 %87.97 - 91 %Balance
Vanadium, V 3.5 - 4.5 %3.5 - 4.5 %
Yttrium, Y <= 0.0050 %<= 0.0050 %
 
Descriptive Properties
Surface roughness20-50 µmRz, after shot peening
 5 - 9 µmRa, after shot peening
Volume rate5 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS957 / 280617

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.