MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trelleborg Horda Cable E8561 Strippable Semiconductive Shielding
Categories: Polymer; Thermoset

Material Notes: E8561 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.

E8561 meets these requirements, when optimal processing, extrusion, and end testing procedure are used:
AEIC-CS8
BS 6622
IEC 60502
NF C 33-223
NEMA WC 7-1996/ICEA S-95-658

All information provided by Horda Cable Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc
@Temperature 23.0 °C
0.0423 lb/in³
@Temperature 73.4 °F
ASTM D1928
Mooney Viscosity 17 - 21
@Temperature 121 °C
17 - 21
@Temperature 250 °F
ISO 289
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85 - 9085 - 90ASTM D2240
Tensile Strength, Yield 11.7 MPa1700 psiafter aging 1 week @ 135°C; ASTM D638
 13.0 MPa1890 psiASTM D638
Elongation at Break 140 %140 %after aging 1 week @ 135°C; ASTM D638
 200 %200 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  <= 500 ohm-cm
@Temperature 23.0 °C
<= 500 ohm-cm
@Temperature 73.4 °F
ASTM D257
 <= 1000 ohm-cm
@Temperature 90.0 °C
<= 1000 ohm-cm
@Temperature 194 °F
ASTM D257
 <= 1000 ohm-cm
@Temperature 120 °C
<= 1000 ohm-cm
@Temperature 248 °F
ASTM D257
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 60.0 - 110 °C140 - 230 °F
Head Temperature 100 - 130 °C212 - 266 °F
Screw Cooling Temperature 40.0 - 50.0 °C104 - 122 °F
Drying Temperature <= 40.0 °C<= 104 °F
Moisture Content <= 0.080 %<= 0.080 %QAHC-10420 (Karl Fischer method)
 
Descriptive Properties
Hot Set (%)70/20200°C, 20 N/cm²; IEC 540
Insulation Shield Stripping Force (N/cm)20-30@ 90°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding
Top Polymer Topolymer® 9210-651 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-751 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-801 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-851 Thermoplastic Vulcanized Elastomer

PTRELL005 / 83763

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.