MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.

LDPE 1022 FH 24 is a slip and anti-block formulated grade.

LDPE 1022 FH 24 is suited to many applications in the field of consumer, industrial, food or hygiene packaging such as bags, lamination and coextrusion film.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.923 g/ccISO 1183
Thickness 40.0 micronsfor samples tested on this data sheet
 20.0 - 150 micronspossible range, depending on extrusion conditions
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Antiblock Level 750 ppmTalc
Slip Level 750 ppmErucamide
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 11.5 MPaISO 527-3
Film Elongation at Break, MD 350 %ISO 527-3
Film Elongation at Break, TD 580 %ISO 527-3
Elmendorf Tear Strength, MD 7.30 g/micronISO 6383-2
Elmendorf Tear Strength, TD 6.10 g/micronISO 6383-2
Dart Drop Test 95.0 gISO 7765-1
Film Tensile Strength at Break, MD 22.0 MPaISO 527-3
Film Tensile Strength at Break, TD 20.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 109 °CISO 11357
Vicat Softening Point 94.0 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %ISO 14782
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 190 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
Braskem F0421 D LDPE Blown Film Extrusion Polyethylene
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene

PTOTAL714 / 130439

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.