  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kumho-Sunny HAM8580 PMMA/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded; Acrylic (PMMA)

Material Notes: HAM8580 is paint free improved PMMA/ABS resin. HAM8580 has comprehensive properties: (1) anti-scratch, PH=2H (2) high gloss (G60°>95) (3) super weather resistance (4) free style (black and spark, semi-transparent, spark, transparent) (5) high without-gap tendity. HAM8580 is mainly used in auto exterior, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 4.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.5 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 65.0 MPa9430 psiASTM D638
Elongation at Break 16 %16 %ASTM D638
Flexural Strength 80.0 MPa11600 psiASTM D790
Flexural Modulus 2.60 GPa377 ksiASTM D790
Izod Impact, Notched 0.450 J/cm
@Thickness 3.20 mm
0.843 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FASTM D648
Vicat Softening Point 105 °C221 °FB; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 220 °C410 - 428 °F
Middle Barrel Temperature 220 - 230 °C428 - 446 °F
Front Barrel Temperature 240 - 260 °C464 - 500 °F
Nozzle Temperature 230 - 250 °C446 - 482 °F
Melt Temperature 235 - 245 °C455 - 473 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Back Pressure 1.00 - 5.00 MPa145 - 725 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKMSN198 / 281050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.