Silver Ink C70709D21 is designed as a top coat for Silver Zinc Ink C70709D22 when printed on PTC ceramics. The C70709D22 should be dried and coated with the C70709D21 before the final drying and firing. The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. Information provided by Gwent Electronic Materials Ltd. |