MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Polynt DISTITRON® 186 Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, Isophthalic

Appearance: Yellow - Transparent

Main resin characteristics: Clear, unaccelerated, Type 1140 (DIN 16946-2), Type UP 2 (DIN 18820-1)

Main applications: BMC and SMC manufacture, very good mechanical properties

Molding information: Hot press molding

Curing cycle: 24h at 23°C + 2h at 100°C + 1h at 100°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Solids Content 64 - 68 %64 - 68 %MT-CU001C
Brookfield Viscosity 2450 - 2850 cP2450 - 2850 cPsp 3 rpm 20; MT-CUT25V
 
Chemical PropertiesMetricEnglishComments
Acid Value 10 - 1710 - 17[mgKOH/g]; MT-CU001I
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4646ASTM D 2583
Tensile Strength 60.0 MPa8700 psiISO 527
Elongation at Break 1.8 %1.8 %ISO 527
Tensile Modulus 3.90 GPa566 ksiISO 527
Flexural Strength 120 MPa17400 psiISO 178/B
Flexural Modulus 3.80 GPa551 ksiISO 178/B
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 113 °C235 °FISO 75 -2A
Glass Transition Temp, Tg 117 °C243 °FASTM E 1545
 
Processing PropertiesMetricEnglishComments
Cure Time 2.67 - 3.33 min
@Temperature 130 °C
0.0445 - 0.0555 hour
@Temperature 266 °F
Reactivity, at 130°C + 1% TBPB; RS.08.G
Shelf Life 6.00 Month6.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm220-260°CRS.08.G; Reactivity, at 130°C + 1% TBPB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9296 / 231891

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.